Din 17243 Pdf Jun 2026
Typical minimum yield strength is approximately 250 MPa ( psi), with a tensile strength ranging from 485 to 660 MPa .
The standard is most famous for defining the requirements for two specific categories of steel:
Guidelines on the allowable deviations for forged and rolled parts.
The standard was officially withdrawn and has been largely replaced by the series (specifically DIN EN 10222-2 ) for steel forgings for pressure purposes. Material (DIN 17243) Material Number Common ASTM Equivalent Accessing the PDF DIN 17243 - 1987-01
Your correct path forward is:
: Requirements for hardness testing to ensure product homogeneity and protocols for long-term creep tests. Heat Treatment
These steels were prized for their ability to withstand repeated loading without permanent deformation. The 50CrV4 (1.8159) grade, for instance, became the gold standard for automotive leaf springs and coil springs.
If you are tracking down a for modern projects, you must reference the exact modern counterparts dictated by standard replacement pathways:
| Source | Format | Cost (approx.) | Notes | |--------|--------|----------------|-------| | (formerly Beuth) | PDF (watermarked) | €90–120 | Official, searchable, correct | | ANSI Webstore (USA) | PDF | $100–130 | Export-controlled, valid for reference | | Techstreet | PDF | ~$110 | Same as DIN Media reseller | din 17243 pdf
Products manufactured under this standard are designed for environments where both high pressure and high heat are constant factors. Common applications include:
: Applies to various grades of ferritic and martensitic steels with specified elevated temperature properties. Common Grade
: Raw stock converted into high-stress studs, bolts, and specialized high-temperature fasteners.
: Primarily used in steam boiler plants, pressure vessels, pipework, and similar high-pressure or high-heat components. Key Materials : Commonly specified grades included (Material No. 1.0460), which is now typically replaced by Current Status & Replacement Typical minimum yield strength is approximately 250 MPa
The DIN 17243 standard is published in a PDF format, which provides detailed information on the technical requirements, testing methods, and quality assurance procedures. The PDF document includes:
Guidelines on finishing, surface defects allowed, and non-destructive testing (NDT) requirements.
Subscribers to engineering databases like IHS Markit or similar platforms often have access to these documents.